Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL GTX™ Resin GTX975 - Americas - (PPE+PA*)-MF18 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL GTX™ Resin GTX975 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl GTX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
NORYL GTX™ 975 resin is a conductive, 18% mineral reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade combines high stiffness and excellent temperature resistance with conductivity for primerless electrostatic painting. NORYL GTX975 was designed for in- or on-line painted exterior automotive trim parts such as tank flaps and corner panels.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 10 cm³/10min ISO 1133
温度 280 °C -
荷重 5 kg -
ASTM数据
メルトフローレイト, MFI 15 g/10min ASTM D 1238
温度 280 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 4200 MPa ISO 527
降伏応力 65 MPa ISO 527
降伏ひずみ 3.5 % ISO 527
破壊応力 65 MPa ISO 527
破壊ひずみ 4 % ISO 527
曲げ弾性率 4000 MPa ISO 178
シャルピー衝撃強さ, +23°C 40 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30゚C 35 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 3 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30゚C 3 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm 40 kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm 35 kJ/m² ISO 180/1U
ノッチ付きアイゾット衝撃強さ, +23°C, 4mm 4 kJ/m² ISO 180/1A
ノッチ付きアイゾット衝撃強さ, -30°C, 4mm 4 kJ/m² ISO 180/1A
ASTM数据
引張弾性率 4450 MPa ASTM D 638
降伏応力 69 MPa ASTM D 638
破壊応力 68 MPa ASTM D 638
降伏点伸び 3.5 % ASTM D 638
破断伸び 4.5 % ASTM D 638
曲げ弾性率 4000 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 35 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 30 J/m ASTM D 256
温度 -30 °C -
熱的特性単位テスト基準
ISO データ
ビカット軟化温度, B 195 °C ISO 306
ビカット軟化温度, 120°C/h 50N 200 °C ISO 306
線膨張係数, 平行 50 E-6/K ISO 11359-1/-2
線膨張係数, 直角 65 E-6/K ISO 11359-1/-2
ASTM数据
DTUL @ 66 psi 210 °C ASTM D 648
ビカット軟化温度 215 °C ASTM D 1525
その他の特性.単位テスト基準
吸水率. 3.5 % Sim. to ISO 62
吸湿率 1.1 % Sim. to ISO 62
密度. 1200 kg/m³ ISO 1183
密度 1250 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 100 - 110 °C -
Pre-drying - Time 2 - 3 h -
Processing humidity ≤0.02 % -
樹脂温度 280 - 300 °C -
金型温度 100 - 120 °C -
Feed temperature 80 - 100 °C -
Zone 1 260 - 280 °C -
Zone 2 270 - 290 °C -
Zone 3 280 - 300 °C -
特殊な特性
成形加工法.
射出成形.
アプリケーション
自動車
領域別の利用可能性
北アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com